The short answer is yes, nylon (PA6 and PA66) can be ultrasonically welded — but it is much harder than ABS. Nylon is a semi-crystalline plastic with a sharp melting point: once melted, it resolidifies almost the moment the temperature drops. Worse, it loves moisture, and a damp part welds into a bubbly, whitish, weak joint. Welding nylon comes down to three things: use a shear joint, keep the parts dry, and validate with a trial weld.

1. Why is nylon hard to weld?

The difference from ABS is crystallinity. Amorphous plastics like ABS soften gradually, but nylon melts at a defined point and freezes again almost instantly, so the melted plastic can solidify before it has fused with the other side — which is why an ordinary energy-director joint works poorly on nylon. Nylon is also hygroscopic: parts left in a warehouse absorb moisture from the air, and at the weld zone the temperature is high enough to flash that moisture into steam, leaving bubbles in the joint and a foamy white bond. According to industry guidelines, exposing nylon parts to air at 23 °C and 50 percent relative humidity for 24 hours can seriously degrade a weld.

2. Use a shear joint, not an energy director

For engineering plastics such as nylon, industry guidelines recommend the shear joint. The two halves telescope together with a small radial interference, so the vibration first melts the contacting edge and then keeps melting along the vertical walls as the parts slide together — the melt stays continuous instead of freezing mid-way. Industry references give a rule of thumb of about 0.3–0.45 mm of interference per side for parts under 40 mm in outside diameter, with a telescoping depth of roughly 1.0–1.5 times the wall thickness; the exact dimensions depend on part size and wall thickness. One more rule: weld nylon only to itself — PA6 to PA6, PA66 to PA66 — not across grades.

3. Drying comes first

Ideally nylon parts are welded in the dry-as-moulded state, with about 0.2 percent moisture recommended for PA66. If immediate welding is not possible, store the parts sealed in aluminium foil bags with desiccant, or oven-bake them at about 80 °C before assembly; the resin itself should also be dried to below 0.15 percent moisture before any heat joining. In short, the longer a nylon part sits around absorbing moisture, the worse the weld — drying is not a step to skip.

4. Large parts can use hot plate welding

Besides ultrasonic welding, nylon can also be joined by hot plate, vibration and spin welding. For larger, thicker-walled nylon parts, where ultrasonic energy cannot reach the whole weld line, hot plate welding is the safer choice. Whichever process is chosen, validate it with a trial weld on the actual material and joint, check pull strength and the fracture surface, and only then fix the process. If you are selecting welding equipment for nylon parts, feel free to contact Shanghai Jingjin for a free welding sample test.