Principle of Ultrasonic Plastic Welding:
Plastic ultrasonic welding is a heat-joining method that uses ultrasound to rapidly fuse the molecules at the contact surfaces of plastic parts. It offers short cycle time, no surface damage, no heating of non-weld areas, no pretreatment, and simple operation, and has been widely applied in aerospace, instrumentation, food packaging, the electronics industry, and more.
Effect of Weld Time on the Heat-Seal Strength of Welded Joints:
During ultrasonic welding, the temperature generated at the weld interface is proportional to weld time. As weld time increases, the temperature produced at the two contact interfaces of the inner layer of the composite film rises; the higher the temperature, the more plastic melts at the interface, the more fully the upper and lower surfaces bond under pressure, and the more thoroughly the molecular chains entangle in the molten region — macroscopically, the heat-seal strength of the welded joint increases. However, excessively long weld time reduces the heat-seal strength of the joint. On the one hand, excessive heat enlarges the heat-affected zone and makes thermal stress concentration at the edges more pronounced, so the weld edges fracture easily. On the other hand, since the film is only tens of microns thick, excessive heat conducting longitudinally can easily affect the properties of the composite film itself, disordering the originally oriented outer-layer film material. In composite films, polyethylene has a lower melting point and a larger loss modulus than polypropylene, so it can generate the energy needed to melt the weld interface in a shorter time, requiring a shorter weld time.
Effect of Weld Pressure on the Heat-Seal Strength of Welded Joints:
For composite films, there is an optimum weld pressure. The heat-seal strength of the welded joint first rises rapidly with increasing weld pressure, then falls rapidly once the pressure exceeds 150 N. This is because low weld pressure cannot bring the contact surfaces into intimate contact, leaving large air regions; under a given period of ultrasound, most of the ultrasonic vibration is lost in the air, interfacial frictional heating is insufficient, the fused region forms unevenly, and the joint's heat-seal strength is low. Once the weld pressure reaches a certain value, the interface can be considered tightly bonded and the interface temperature rises rapidly. Pressure promotes diffusion of polymer chains, forming a dense structure in the weld zone, and the heat-seal strength increases within a certain range. But if the weld pressure is too high, the molten polymer is extruded and flows faster, polymer chains align laterally along the weld surface, thermal stress concentration at the edges intensifies, and brittle fracture of the weld edges occurs. In addition, as weld pressure increases, the metal horn edges can easily damage the film, causing a sudden drop in heat-seal strength.
Ultrasonic Welding Process for Plastic Composite Films:
1) Within a suitable weld amplitude range (5 μm–7 μm), polyester/polypropylene composite films achieve high welded-joint heat-seal strength. When a polyethylene with a larger loss modulus is used as the inner layer of the composite film, the influence of weld amplitude on the joint's heat-seal strength diminishes.
2) As weld time increases, the heat-seal strength of both composite films' welded joints first rises and then falls. When the composite film reaches its maximum welded-joint heat-seal strength, the lower-melting-point polyethylene-based composite film requires less time than the polypropylene-based composite film.
3) When the weld pressure is about 150 N, both composite films' welded joints reach their maximum heat-seal strength.
4) The welded-joint heat-seal strength of polyester/polyethylene composite film is higher than that of polyester/polypropylene composite film.