(1) First connect the ultrasonic equipment's working air source and make sure the air pressure gauge reads normally.
(2) Using the dedicated wrench, remove the existing welding tooling from the machine and install the ultrasonic tooling for the product to be welded (clockwise loosens — remember it must be tightened securely). Note: tighten the tooling screws first.
(3) Connect the ultrasonic equipment to power, switch on the start button and wait five seconds, then switch off. Immediately press the sound test button on the controller; you should hear the machine emit ultrasound (the sound should be crisp, free of hoarseness and extraneous noise). If the sound is hoarse or screeching, check the tooling for cracks or looseness and take corrective action.
(4) Loosen the two locking handles at the back of the machine frame and crank the machine head up to a suitable height (depending on product height).
(5) Shut off the air supply. (Adjust the air pressure controller to "zero".)
(6) Place the product to be welded on the bottom tooling and make sure the molds close properly.
(7) Pull down the vibrator barrel so the upper tooling approaches the bottom tooling, then crank the head lifting mechanism so the upper tooling presses onto the product, keeping the product fitted to both the upper and lower tooling.
(8) Raise the air pressure to 0.1 MPa, set the selector switch to manual, and press the two green start buttons so the tooling descends and presses the product.
(9) Crank the lifter so the limit screw and the vibrator barrel stay 1 mm apart (adjust for the product being welded).
(10) Tighten the frame locking handles, fix the bottom tooling in place, and press the red emergency stop button so the machine head rises.
(11) Set the selector switch to auto, adjust the product's welding parameters and time, and get ready for production.
If during production the product welds unevenly or shifts, adjust the leveling nuts to correct it. Leveling example {If the welded product shows over-melting (too heavy) with flash
on the right side and under-melting (too light) on the left, make the following adjustment. Apply the same logic to similar cases.}
PreviousSeawater Desalination Membrane Welder Operating ProceduresNextUltrasonic Spot Welder Operating Process