Ultrasonic staking: 
    A variation of ultrasonic welding is ultrasonic staking: a method of fastening a thermoplastic part to a part of a different material. The stud or boss should have a very generous radius or fillet at its base to prevent cracking or melting. To concentrate ultrasonic energy, the top of the boss should be designed for minimal initial contact with the horn. The boss top may be flat or conical; conical is preferred for semi-crystalline or filled polymers. The integrity of ultrasonic staking depends on the precise volumetric relationship between the stud and the horn. 
    Standard staking: flat-head studs with diameters between 1.6 and 4.0 mm. The standard profile is recommended for rigid and flexible non-abrasive thermoplastics. 
    Hemispherical staking: studs under 1.6 mm in diameter are recommended for hemispherical staking. Suitable for abrasive plastics. 
    Flush staking: used in applications requiring a flat or raised surface where the thickness of the mating part permits. 
    Hollow staking: bosses or studs larger than 4 mm in diameter can be cored to form blind-hole bosses. 
    When through-holes are not permitted in the mating parts, ultrasonic welding equipment can also form a mechanical interlock. Molded plastic studs (similar to those used in staking) and blind chamfers in the mating parts create a true tolerance-based mechanical joint (assuming the chamfered part does not melt).  
    1. Amorphous polymers—especially those in the glassy state at room temperature—are generally good candidates for welding processes. Glassy amorphous polymers have good transmissivity, allowing successful welding with both near-field and far-field techniques. When the material is soft, ultrasonic welding of amorphous materials becomes problematic; e.g., welding high-impact PS generally requires more energy and additional amplitude than welding general-purpose PS. 
    2. Semi-crystalline polymers are generally harder to weld with ultrasonic energy. Increase the energy delivered by the welding system (i.e., increase amplitude); shorten the distance between the horn/part contact surface and the joint interface; use near-field ultrasonic welding; use horns with amplitudes up to 0.05–0.15 mm. These high welding amplitudes require titanium horns. When high-strength, sealed assemblies are needed, shear joints and scarf joints both suit semi-crystalline polymers. 
    3. Welding hygroscopic polymers: weld parts immediately after molding (while still dry); dry parts before welding; store parts in a desiccator before welding.