Common Problems in Ultrasonic Welding: 
    Improper weld parameter settings: ultrasonic operating conditions mean the settings of machine output power (amplitude steps), pressure (dynamic force vs. static pressure), weld time, hold time, delay time, and other parameters.  Take the ultrasonic energy director as an example. When we perform ultrasonic welding, if the pressure is too high and the cylinder descends with too little cushioning, the energy director is easily flattened. Although the product may look sealed, the energy director has been squeezed and sunk, losing its energy-directing
   effect; instead of a guided weld at the triangular points, the result is a forced face-to-face weld of the plastic — a false weld.
    Insufficient ultrasonic energy output: when buying an ultrasonic welder, customers can rarely predict future product specifications, so they may face jobs beyond the standard capacity of the machine. With no budget to add equipment, they must produce with what they have. Facing this kind of small-machine-big-job situation, common approaches are multiple weld passes, higher ultrasonic output power (more amplitude steps), or longer weld time and higher pressure. But this also creates unstable quality, because voltage and air pressure directly affect the stability of ultrasonic output power. In other words, parts welded during working or peak hours differ in quality from parts welded after everyone has gone home. But running ultrasonic welding only after hours is hardly efficient. The remedies are: use an independent air supply; 0.02m/m  and for products toleranced below it, fit the ultrasonic machine with a voltage stabilizer; adjust the amplitude steps and increase power — though under normal conditions ultrasonic output power is best kept between 2~4 steps; if operation at 5~6 steps is unavoidable, keep production runs as short as possible to avoid wearing out parts and the vibrator. Increasing the gain of the booster (the upper horn mold) helps too. But if the gain exceeds 4:1, it greatly affects the horn itself, the sound waves, and the current.
    Unstable weld quality : the main reason quality cannot stay stable is unstable output power, which prevents the formation of steady frictional heat.