| What Is Ultrasonic Staking Technology:
A variation of ultrasonic welding is ultrasonic staking — a method of fastening a thermoplastic part to a part of a different material. Studs or bosses should have a generous radius or fillet at the base to prevent cracking or melting. To concentrate ultrasonic energy, the top of the boss should be designed for minimal initial contact with the horn. The boss top can be flat or conical; conical is better for semi-crystalline or filled polymers. The integrity of ultrasonic staking depends on the precise fit between the stud and the horn.
Standard staking – flat-head studs 1.6–4.0mm in diameter. The standard profile is recommended for rigid and flexible abrasion-resistant thermoplastics.
Dome staking – studs under 1.6mm in diameter are recommended for dome staking. Suitable for abrasion-resistant plastics.
Flush staking – used where a flat or raised surface is required and the thickness of the locking part allows it.
Hollow staking – bosses or studs over 4mm in diameter can form blind-hole bosses after coring.
Where through-holes are not allowed in the mating parts, ultrasonic welding equipment can still form a mechanical interlock. Molded plastic studs (similar to those used for staking) and blind chamfers in the mating parts create a true tolerance-based mechanical joint (assuming the chamfered part does not melt).
Material Factors in Ultrasonic Welding:
1. Amorphous polymers, especially those that are glassy at room temperature, are usually good candidates for the welding process. Glassy amorphous polymers transmit well, allowing successful near-field and far-field welding. When the material is softer, ultrasonic welding of semi-crystalline materials becomes problematic. For example, welding high-impact PS generally needs more energy and additional amplitude than welding general-purpose PS.
2. Semi-crystalline polymers are generally harder to weld with ultrasonic energy. Increase the energy emitted by the welding system (i.e., increase amplitude); shorten the distance between the horn/part contact face and the joint interface; use near-field ultrasonic welding; use horns with amplitudes up to 0.05–0.15mm. These high welding amplitudes require titanium horns. Shear joints and scarf joints both suit semi-crystalline polymers where high-strength, sealed assemblies are needed.
3. Welding hygroscopic polymers: weld parts right after molding (while still dry); dry parts before welding; store parts in a desiccator before welding.
|