ABS — acrylonitrile-butadiene-styrene copolymer 
    Chemical and physical properties:
    ABS is synthesized from three chemical monomers: acrylonitrile, butadiene, and styrene. Each monomer has distinct characteristics: acrylonitrile provides high strength, thermal stability, and chemical stability; butadiene provides toughness and impact resistance; styrene provides easy processability, high gloss, and high strength. Morphologically, ABS is a non-crystalline material. Polymerization of the three monomers produces a two-phase terpolymer: a continuous styrene-acrylonitrile phase and a dispersed polybutadiene rubber phase. The properties of ABS depend mainly on the ratio of the three monomers and the molecular structure within the two phases. This gives product designers great flexibility and has produced hundreds of different grades of ABS on the market. These different grades offer different properties, from medium to high impact resistance, from low to high gloss and high heat-deflection characteristics. ABS offers superb processability, appearance, low creep, excellent dimensional stability, and very high impact strength.
    Injection molding process conditions: 
    Drying: ABS is hygroscopic and must be dried before processing. Recommended drying conditions are at least 2 hours at 80–90 °C. Material moisture should be kept below 0.1%. Melt temperature: 210–280 °C; recommended temperature: 245 °C. Mold temperature: 25–70 °C. (Mold temperature affects part gloss — lower temperature means lower gloss.) Injection pressure: 500–1000 bar. Injection speed: medium-high speed.
    Typical uses:
    Automotive (instrument panels, tool compartment doors, wheel covers, mirror housings, etc.), refrigerators, high-strength tools (hair dryers, mixers, food processors, lawn mowers, etc.), telephone housings, typewriter keyboards, recreational vehicles such as golf carts and snowmobiles.