Common Defects in Non-Woven Bag Welding and How to Fix Them

Ultrasonic lace machines weld non-woven bags fast and need no preheating, but real production still runs into weld defects. Knowing what causes them helps you adjust the process quickly and keep quality stable.

1. Cracked or weak seams
Usually caused by insufficient welding energy or low pressure. Try raising the amplitude, extending weld time, or checking whether the horn surface is worn and the pattern roller engraving has shallowed. Always pull-test a few samples before mass production.

2. Scorched or burned-through fabric
Mostly from excessive energy or dwell time. Lower the amplitude setting, speed up feeding, and check that the pattern roller is aligned with the horn. Fabrics of different weights need their own parameter sets — one setting does not fit all.

3. Uneven seam width or blurred patterns
Typically the pattern roller is not parallel to the horn, or feeding tension is uneven. Re-calibrate roller parallelism, keep feeding steady, and regularly clean melt residue off the horn surface.

4. Routine maintenance
Pattern rollers and horns are wear parts: clean off residue after production and check that the roller teeth are intact. For long shutdowns, apply a light coat of rust-preventive oil on the roller. Keep the machine clean and log your parameters — complete records let you dial in the right settings quickly next time you change material.

A tip from our engineers: after changing material or pattern rollers, always run a few test pieces first. Confirming the weld before full production cuts scrap dramatically.