Chemical name: Acrylonitrile-Butadiene-Styrene copolymer 
  English name: Acrylonitrile Butadiene Styrene (ABS)
  Applications: automotive parts (instrument panels, tool compartment doors, wheel covers, mirror housings, etc.), radio housings, telephone handsets, heavy-duty tools (vacuum cleaners, hair dryers, mixers, lawn mowers, etc.), typewriter keyboards, recreational vehicles such as golf carts and snowmobiles, etc.
  Specific gravity: 1.05 g/cm³ 
  Burn test: burns continuously, blue-based yellow flame, black smoke, faint marigold odor
  Solvent test: cyclohexanone softens it; aromatic solvents have no effect
  Drying conditions: 80–90 °C for 2 hours
  Molding shrinkage: 0.4–0.7% 
  Mold temperature: 25–70 °C (mold temperature affects part surface finish; lower temperatures produce lower gloss)
  Melting temperature: 210–280 °C (recommended: 245 °C)
  Molding temperature: 200–240 °C 
  Injection speed: medium-high
  Injection pressure: 500–1000 bar
  Characteristics: 
  1. Good overall performance, high impact strength, chemical stability, and good electrical properties. 
  2. Welds well with #372 acrylic; can be made into two-color parts and can be chrome-plated or painted. 
  3. Available in high-impact, high-heat, flame-retardant, reinforced, and transparent grades. 
  4. Flowability slightly lower than HIPS but better than PMMA, PC, etc.; good flexibility. 
  5. Applications: suitable for general mechanical parts, anti-friction and wear-resistant parts, transmission parts, and telecommunications parts. 
  6. Like PVC, whitening occurs at bends.
  Molding characteristics: 
  1. Amorphous material with medium flowability and high moisture absorption; must be thoroughly dried. Parts requiring a glossy surface need extended pre-drying at 80–90 °C for 3 hours. 
  2. Use high melt and mold temperatures, but excessive melt temperature causes decomposition (decomposition temperature >270 °C). For high-precision parts, mold temperature should be 50–60 °C; for high-gloss, heat-resistant parts, 60–80 °C. 
  3. To eliminate weld lines, improve material flowability by using high melt/mold temperatures or changing the gate location. 
  4. When molding heat-resistant or flame-retardant grades, plastic decomposition residues remain on the mold surface after 3–7 days of production, causing the mold surface to become shiny; clean the mold promptly and add venting to the mold surface. 
  ABS resin is currently the highest-volume, most widely used polymer, organically combining the properties of PS, SAN, and BS with well-balanced toughness, hardness, and rigidity. ABS is a terpolymer of acrylonitrile, butadiene, and styrene—A stands for acrylonitrile, B for butadiene, and S for styrene. 
  ABS engineering plastic is generally opaque, light ivory in appearance, non-toxic and odorless, combining toughness, hardness, and rigidity. It burns slowly with a yellow flame and black smoke; after burning, the plastic softens and chars, emitting a distinctive cinnamon odor, but with no molten dripping. 
  ABS engineering plastic offers excellent overall performance: outstanding impact strength, good dimensional stability, electrical properties, wear resistance, chemical resistance, and colorability, plus good moldability and machinability. ABS resin resists water, inorganic salts, alkalis, and acids; it is insoluble in most alcohols and hydrocarbon solvents, but readily soluble in aldehydes, ketones, esters, and certain chlorinated hydrocarbons. 
  Drawbacks of ABS engineering plastic: low heat-deflection temperature, flammable, and poor weather resistance.