1. Setting the trigger time: this should be determined by the travel and speed of the descending ultrasonic die (horn). The goal is for the ultrasonic die (horn) to emit ultrasound the instant before it touches the plastic part while descending. 
    2. Setting the weld time: this is determined by the "pressure used to clamp the plastic part" and the "weld result"; {for example: 1. If plastic "splashes out as flash" at the weld interface, it means the "weld time" is too long, the pressure is too high, or the "down-travel adjustment (limit) screw" is set too low; if the weld interface is insufficiently melted, the opposite is true. 2. If the weld interface melts unevenly along its length, it means the pressure varies along its length — this may be due to low pressure combined with significant plastic part deformation; try increasing the pressure, or the "ultrasonic anvil" may not be mating the two halves of the plastic part completely, in which case adhesive tape can be used to shim the under-melted areas of the "ultrasonic anvil" higher, testing repeatedly to achieve the best weld result}. 
    3. Special attention: with "weld time" and the position of the "down-travel adjustment (limit) screw" unchanged, adjusting the air pressure value of the pneumatic valve can also change the weld result. Therefore, during normal use, the air supply pressure must be kept higher than the set pressure value. 
    4. Setting the pressure (cooling) time: if the plastic part shows "no deformation", "no internal stress after welding" and "solidification is not very slow", usually no cooling time value is selected (or only 1/5 second).
    Trigger early; don't drag out the weld; keep cooling as short as possible. Preliminarily select a weld time [of about 0.3 seconds] and a hold-pressure (cooling) time [of 0 seconds — except for slow-solidifying plastics].