Features of the Hot Plate Plastic Welding Machine:
    The equipment series is available with vertical or parallel hot plate arrangements, and the drive system uses pneumatic, hydraulic, or servo motor drive in a flexible design to suit production needs.  
    Advantages of the Hot Plate Plastic Welding Machine:
    It can be applied to workpieces of different sizes with no area limitation, and to any weld surface with no special requirements. It allows compensation of plastic flash and guarantees weld strength. The welding program can be adjusted to the needs of various materials. Equipment specifications: hot plate welding tooling moves horizontally or vertically; equipment size depends on the size of the parts being welded; the drive method can be pneumatic, hydraulic, or servo motor depending on equipment size; semi-automatic or fully automatic mode can be selected per welding program requirements. The equipment maintains good stability, ensuring consistent weld results and accurate workpiece height after processing. Welding temperature, heating time, cooling time, heating depth, melt depth, pressure, transfer time, and other parameters are all adjustable, as are other optional welding parameters. On machines with a horizontal hot plate design, the hot plate can rotate 90° for cleaning.  
    DSM thermoplastics can be hot plate welded — the process even suits very soft materials like Arnitel, but is less suitable for Akulon PA66 and Stanyl. Due to oxidative degradation of the molten polymer, it is difficult to obtain satisfactory weld strength with PA66. Stanyl has very low melt viscosity and tends to drip. One of the main advantages of hot plate welding is that it can join dissimilar materials, such as amorphous and semi-crystalline polymers, or polymers with very different melting points. The recommended hot plate temperature depends largely on the specific thermoplastic. Amorphous plastics require 100°C–160°C (212°F–320°F) above the glass transition temperature (Tg). The optimum welding temperature for semi-crystalline materials is 40°C–100°C (100°F–210°F) above the melting point (Tm). The hot plate is often coated with PTFE to prevent parts from sticking to it. In that case, the hot plate temperature should be limited to 260°C, because PTFE begins to vaporize at 270°C–275°C. The maximum temperature of a hot plate without PTFE is 450°C.
    PTFE-Coated Hot Plates Have the Following Characteristics:
    Parts stick less to the hot plate;   
    Lower temperature means less polymer degradation;  
    Lower temperature means a longer weld cycle;  
    PTFE coating has a limited service life. Selecting a higher hot plate temperature can sometimes prevent parts from sticking. High-temperature hot plate welding of PC should be performed above 300°C. Non-contact welding is another way to prevent sticking: here a small gap separates the plastic part from the hot plate, and heat is transferred by radiation rather than conduction, so the hot plate temperature must be set higher — up to 450°C can be used. In non-contact welding, oxidative degradation of the molten surface occurs more readily, reducing weld strength. High temperatures up to 450°C can be used for non-contact welding and to shorten the weld cycle, but oxidation of the molten surface easily reduces weld strength. For hot plate welding without a PTFE coating, temperatures above 300°C are used to prevent parts from sticking. Careful control of the relative displacement of the parts and the welding pressure is very important. If the welding pressure is too high, the molten polymer will be completely squeezed out of the joint and weld strength will be very low. The two basic principles for controlling weld penetration are "pressure-controlled welding"  and "distance-controlled welding." In the first type, pressure is controlled throughout the process. But the most commonly used control principle is distance-controlled welding, which uses rigid mechanical stops to control dimensions. The changeover time from polymer melting to part assembly should be as short as possible to avoid premature cooling and to melt the oxide film as much as possible.